Brand Name : UNICOMP
Model Number : UNZ-450
Certification : CE
Place of Origin : China
MOQ : 1Set
Price : can negotiate
Payment Terms : T/T, L/C
Supply Ability : 10 sets per month
Delivery Time : 30 days
Packaging Details : Wooden Case, Waterproof, Anti-collision
Name : X-ray Inspection Machine
Application : Aluminum Casting, Iron Casting, Auto Parts, Wheels, Metal Products, Refractory Materials
Tube Voltage : 450KV (160KV, 225KV, 320KV for option)
X-ray Leakage : < 2.5uSv/h
Weight : 17.5 T
Power Consumption : 10 kW
Casting defects heat sinks, hot tears, cold-flow, drag-marks, missing material and cracks NDT X-Ray Inspection
Application Fields of X Ray Machine UNZ-450
● Engineering components
● Small aluminum castings, iron castings
● Auto parts, metal products
Technical Parameters and Specifications of X Ray Machine UNZ-450
System Parameters | |
Dimensions | 2766mm*2813mm*2598mm(L*W*H) |
Equipment weight | 17.5T |
Power | 10 kW |
Maximum penetration (FE) | 80 mm |
Detection range | Φ550*200mm |
Load weight | 30kg |
Work environment | 5-40° ≤80%HR |
Power supply | Three-phase five wire system AC380V |
X-ray leakage dose rate | ≤2.5μSv/h |
X-ray Generator | |
Tube voltage | 450KV (160KV, 225KV, 320KV for option) |
Power | 700W / 1500W |
Focal size | 0.5mm |
Detector (FPD) | |
Image area | 250mm×300mm |
Pixel matrix | 1792×2176 |
Pixel pitch | 139μm |
Frame rate | 9fps(1×1) 30 fps(2×2) |
Software Function | |
Image processing | brightness and contrast adjustment; stacking frames, window width and level adjustment; image enhancement, filtering, sharpening, invert, relief and bubble measure;ove, zoom in, zoom out, display image scaling, display the current mouse coordinates and gray values |
Image measurement | distance, radius, polygon, angle measurement; arrows and text labels; save the image after processing |
Motion control | the speed adjustment of each moving axis; CNC programming; manual operation; |
Additional function | |
● CNC programmable control, to save the detection time of the bulk of the workpiece | |
● C type arm five detection mechanism, no dead angle detection | |
● Servo stepper motor drive, stable operation | |
● Voltage regulator, isolation, filtering, grounding and other protective functions are complete | |
● Set aside industrial cloud interface, data and pictures in real time upload, with traceability and large data analysis(optional) |
* Specifications are subject to change without notice, All trademarks are the property of the system maker.
X-Ray Images
Dimensions and Appearance
![]() |
10 KW NDT X Ray Equipment For Casting Defects Heat Sinks / Hot Tears / Cold Flow Images |